ATD and DSC analyses of nickel superalloys
Nickel superalloys ATD analysis DSC analysis Temperature Solidification Microstructure Carbides
2011/3/17
The study presents the results of investigations of phase transformations that take place during melting and solidification of nickel superalloys, like RENE 77, IN7 13C, MAR 247 and IN 100. Examinatio...